Wabi Sabi and Me
Electroform 1.5 liter Super Delux Kit 5A Power Supply & Magnetic Stirrer Bring Your Electroform kit up to the next level for Better Results
Electroform 1.5 liter Super Delux Kit 5A Power Supply & Magnetic Stirrer Bring Your Electroform kit up to the next level for Better Results
READY TO SHIP, I usually ship out sets ASAP.
Most starter sets that I see are 1 AMP and 1 Liter, this set is 5 amps and 1.5 liters, so you'll have a bigger capacity to start with compared to other sets. Plus it comes with advanced freatures such as a magnetic stirrer, anti corrosion titanium hardware and a titanium anode cage, saving you hours of time giving you even better results!
The 5A power supply and other accessories will allow you to eventually go to a larger tank if you want to create even bigger items or start your own small business. In addition this 5AMP power supply works in Constant Current and Constant voltage mode allowing you to expand and do gold plating, silver plating, nickel plating,electro polishing, electro cleaning, electro etching, brush plating, palladium plating, zinc plating , tin plating, small anodizing projects, and electrolytic patinas.
This is a great beginners set it includes pretty much everything needed to start electroforming including a very easy to use power supply.
If you choose the set that includes the copper sulphate, you will only need to supply Sulphuric acid which is readily available in most places and I can help you to source that if needed.
Bring Your Electroform KIt to the next level, get more consistent results. If you purchase this complete kit with power adapter and copper sulphate all you will have to supply is sulphuric acid to start electroforming.
This is the basic Set Upgreaded with A power Supply and a magnetic stirrer.
Kit Includes:
Hardware
1.5 liter container
Power Supply*
Anode Cage
Anode Cage Bag
Magnetic Stirrer
Stir bar
Titanium Bus Bar
Bus Bar Brackets
Cathode Clips
Heavy Duty Power Leads
copper test squares
syringe for dosing chloride and lustro Smooth-O
Coffee Filters
Chems
LUSTRO ELECTRO SUPER BRIGHT. Part A- Red Label – BRIGHTENER
LUSTRO SMOOTH-O MINI Trial Size Part B – Carrier & Leveling agent.
Chloride
Lustro Dip O Protective Dip
Sulphur for making patina
You will need to supply Sulphuric acid.
If you need help sourcing sulphuric acid contact me
Add On items
5A 12 V power adapter ( voltage source for power supply)
Copper Sulphate to make Electroform Solution
FREE Support
Formula for conductive paint
Formula and instructions for electroform solution
Chloride Dosing Instructions
Advice on set and where to get othert items that are needed locally
Electroform Knowledge Club Newsletter
Preparation Of Brightener
Add 50ML heated ( hot but not nearly boiling) distilled water to bottle, replace cap, and shake well until all solids are dissolved.
FOR BEST RESULTS PLEASE DO NOT FILL BOTTLE ONLY ADD 50ML DISTILLED WATER.
Whole batch must be made at same time other wise it will not work properly.
Start by Adding 5 drops per liter to copper sulfate based electroforming solution and then testing. The exact amount needed will be determined by your baths make up. Our customers have reported 5-10 drops per liter were used, start at 5 and work your way up. My baths use between 5-6 drops. Current setting can range from .1A/ in2- .3A/ in2 depending of electroformed project and the composition of your bath. Start low and slowly increase current until bright and shiny surface develops.
Do not mix with other brighteners or leveling agents as they may not be compatible.
For this brightener to work properly chloride is needed in the bath, the easiest way to do this is watch our video on Chloride Dosing.
Lustro Smooth-O
Long Lasting
Treats UP to 5 Liters
Top Up as needed
Fast copper deposition, use with higher current and cut plating times
---------------------------------------------
Preparation of MINI Lustro Smooth-O
Add 8ML heated ( hot) distilled water to bottle, replace cap, and shake well until all solids are dissolved.
FOR BEST RESULTS PLEASE DO NOT FILL BOTTLE ONLY ADD 8ML DISTILLED WATER.
Whole batch must be made at same time otherwise it will not work properly.
Add .5-2ml per liter
Treats up to 5 liters
Top Up when needed
Less topping up than Lustro Electro Superbright
---------------------------------
Check out the Preparation video on Youtube:
Electro Jeweler Jordan
FAQ About Lustro Electro Brightener
https://electrojewelerjordan.com/?page_id=696
@electrojewelerjordan. - Jewelry
@lustroelectro - Electroform Tips and tutorials
YouTube Electrojeweler JOrdan
https://www.youtube.com/channel/UCzOmpfKTlYg4-XghqplaDuQ
Check back as we will be adding many new and innovative products that Electro Jewelers need.
Follow us on Instagram for tips, tricks, jewelry making instruction and special offers:
https://www.instagram.com/lustroelectro/